SAN details
- SAN Unfilled
- SAN Glass Filled
SAN unfilled details
Property | Description |
---|---|
V200 | General purpose |
SAN Unfilled test results
Property | Test Method | V200 |
---|---|---|
Description | General purpose | |
Processing Method | Injection | |
Specific gravity, g/cc | ASTM D792 | 1.07 |
Linear mold shrinkage, in/in(m) | ASTM D955 | .0035(.0035) |
Hardness, Rock well | ASTM D785 | M83 |
Reinforcement content % | ASTM D2584 | - |
Notched izod impact, ft-lb/in(J/m) | ASTM D256 | 0.5 (26.7) |
Tensile strength | ASTM D638 | 10,500 (72.4) |
Elongation, Ultimate % | ASTM D638 | 3 |
Flexural modulus psi (MPa) | ASTM D790 | 500,000 (3448) |
Heat detection temp, @66 psi °F(°C) @264 psi °F(°C) | ASTM D648 | 213(101) 208(98) |
Special Features | Excellent Rigidity Chem. Resist. |
SAN Glass filled details
Property | Description |
---|---|
V350/30 | 30% Glass fiber reinforced |
V350/40 | 40% Glass fiber reinforced |
V200/10 | 10% Glass fiber reinforced |
V200/20 | 20% Glass fiber reinforced |
V200/30 | 30% Glass fiber reinforced |
SAN glass filled test results
Property | Test Method | V350/30 | V350/40 | V200/10 | V200/20 | V200/30 |
---|---|---|---|---|---|---|
Description | 30% Glass Fiber Reinforced | 40% Glass Fiber Reinforced | 10% Glass Fiber Reinforced | 20% Glass Fiber Reinforced | 30% Glass Fiber Reinforced | |
Processing Method | Injection | Injection | Injection | Injection | Injection | |
Specific gravity, g/cc | ASTM D792 | 1.30 | 1.42 | 1.15 | 1.22 | 1.31 |
Linear mold shrinkage, in/in(m) | ASTM D955 | .002(.002) | .002(.002) | .002(.002) | .0015(.0015) | .001(.001) |
Hardness, Rock well | ASTM D785 | R115 | R118 | R121 | R122 | M123 |
Reinforcement content % | ASTM D2584 | 30 | 40 | 10 | 20 | 30 |
Notched izod impact, ft-lb/in(J/m) | ASTM D256 | 1.2 (64.1) | 1.3 (69.4) | 0.7 (37.4) | 1.0 (53.4) | 0.9 (48.1) |
Tensile strength | ASTM D638 | 6,500 (44.8) | 7,500 (51.7) | 11,500 (79.3) | 15,000 (103) | 16,000 (110) |
Elongation, Ultimate % | ASTM D638 | 2 | 2 | 2 | 2 | 1 |
Flexural modulus psi (MPa) | ASTM D790 | 900,000 (6207) | 1,250,000 (8621) | 800,000 (5517) | 1,100,000 (7586) | 1,450,000 (10000) |
Heat detection temp, @66 psi °F(°C) @264 psi °F(°C) | ASTM D648 | 210(99) 190(88) | 220(104) 200(93) | 225(107) 215(102) | 225(107) 215(102) | 225(107) 215(102) |
Special Features | High impact | High impact | High rigidity | High rigidity | Very high rigidity |